| Marke | % Chemische Analyse (%) | Fhysical Eigenschaften | |||||||||
| MgO≥ | SiO2≤ | Fe2O3≤ | CaO≤ | Al2O3≤ | C.C.S (Mpa) | A.P (%) | B.D (g/cm3) | Feuerfestigkeit Unter Last () | 950 Wärmestoß Widerstand (Abkühlen 950air) | C/S | |
| TK-DMZ-98 | 98 | 0.5 | 0.3 | 0.9 | 0.2 | 90 | 14 | 3.2 | 1700 | 25 | 2.0 |
| TK-DMZ-97 | 97 | 0.5 | 0.4 | 1.2 | 0.2 | 90 | 15 | 3.2 | 1700 | 25 | 2.0 |
| TK-DMZ-96 | 96 | 0.6 | 0.6 | 1.3 | 0.2 | 80 | 16 | 3.1 | 1680 | 25 | 2.0 |
| TK-DMZ-95 | 95 | 1.0 | 0.7 | 1.8 | 1.8 | 60 | 16 | 3.0 | 1650 | 20 | |
| TK-DMZ-98 | 98 | 0.5 | 0.3 | 0.6 | 0.2 | 90 | 14 | 3.2 | 1700 | 20 | 1.0 |
| TK-DMZ-97 | 97 | 0.6 | 0.3 | 0.7 | 0.2 | 90 | 15 | 3.2 | 1700 | 20 | 1.0 |
| TK-DMZ-96 | 96 | 0.9 | 0.6 | 1.0 | 0.2 | 80 | 16 | 3.1 | 1680 | 20 | 1.0 |
| TK-DMZ-95 | 95 | 1.5 | 0.7 | 1.5 | 0.3 | 60 | 16 | 3.0 | 1650 | 15 | |
China