Hauptsächlichrohstoff
water based synthetic polymers
Verbrauch
exterior wall paint
Anwendungs-Methode
Elektronikbürste
yield
approx.2 to 4 m2 per l
specific weight
1650 plus minus 100 g per l
viscosity at 20 degrees C
35000 plus minus 5000 cP
drying at 20 degrees C through drying
48 hrs