Ursprungsort
Liaoning, China
Feuerfestigkeit (Grad)
Common (1580°< Refractoriness< 1770°)
Verarbeitung Service
Stanzen, Abwickeln, Schneiden, Moulding
Styles
Different MgO Content & Shapes Accord To Different Using Position
Cold Crushing Strength (MPa)≥
60
Temp Under Load 0.2 Mpa°C
≥1560-1700
Linear Change After Heat At (1650°C, 2h)
0 to -0.4%